Abstract
In contrast to molecular systems, which are defined with atomic precision, nanomaterials generally show some heterogeneity in size, shape, and composition. The sample inhomogeneity translates into a distribution of energy levels, band gaps, work functions, and other characteristics, which detrimentally affect practically every property of functional nanomaterials. We discuss a novel synthetic strategy, colloidal atomic layer deposition (c-ALD) with stationary reactant phases, which largely circumvents the limitations of traditional colloidal syntheses of nano-heterostructures with atomic precision. This approach allows for significant reduction of inhomogeneity in nanomaterials in complex nanostructures without compromising their structural perfection and enables the synthesis of epitaxial nano-heterostructures of unprecedented complexity. The improved synthetic control ultimately enables bandgap and strain engineering in colloidal nanomaterials with close to atomic accuracy. To demonstrate the power of the new c-ALD method, we synthesize a library of complex II-VI semiconductor nanoplatelet heterostructures. By combining spectroscopic and computational studies, we elucidate the subtle interplay between quantum confinement and strain effects on the optical properties of semiconductor nanostructures.
| Original language | English |
|---|---|
| Pages (from-to) | 13487-13496 |
| Number of pages | 10 |
| Journal | Journal of the American Chemical Society |
| Volume | 141 |
| Issue number | 34 |
| DOIs | |
| State | Published - 28 Aug 2019 |
| Externally published | Yes |
Bibliographical note
Publisher Copyright:© 2019 American Chemical Society.
Fingerprint
Dive into the research topics of 'Colloidal Atomic Layer Deposition with Stationary Reactant Phases Enables Precise Synthesis of "digital" II-VI Nano-heterostructures with Exquisite Control of Confinement and Strain'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver