Abstract
Large single crystals, up to 8" diameter, of high quality Optical Germanium, have been grown by the Czochralski technique. Post-growth thermal treatment improves the optical homogeneity and reduces optical losses, as shown by refractive index gradients and MTF measurements. A new approach for the piecewise combination of interferograms as well as a polychromatic treatment of MTF, are presented.
Original language | English |
---|---|
Pages (from-to) | 96-102 |
Number of pages | 7 |
Journal | Proceedings of SPIE - The International Society for Optical Engineering |
Volume | 819 |
DOIs | |